Polymer Property : Tensile Stress = 3488 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 24.05 MPa

@Strain 0.970 %,
Temperature 23.0 °C
3488 psi

@Strain 0.970 %,
Temperature 73.4 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® RS 3061HSL BK039A Nylon 610  (Unverified Data**)
Unreinforced Renewably Sourced Polyamide 610 Developed for Injection Molding Zytel RS 3061HSL BK039A is a renewably sourced polyamide 610 resin containing a minimum of 60% renewably sourced ingredie..