Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 2.37 MPa @Strain 300 % |
344 psi @Strain 300 % |
ASTM D412 |
Polymax® Maxelast® A9955H TPE, ABS/PC Overmold Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesInform.. |
|||
Tensile Stress | 2.37 MPa @Strain 300 % |
344 psi @Strain 300 % |
ASTM D412 |
Polymax® Maxelast® P3855 TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Stress | 2.37 MPa @Strain 0.920 %, Temperature 90.0 °C |
344 psi @Strain 0.920 %, Temperature 194 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® LC6200 BK385 Nylon 612
(Unverified Data**) Toughened Polyamide 612 Developed for ExtrusionInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 2.37 MPa @Strain 0.000 %, Temperature 23.0 °C |
344 psi @Strain 0.000 %, Temperature 73.4 °F |
DAM; ISO 11403-1/-2 |
DuPont Performance Polymers Zytel® PLUS PLS95G50DH2 BK261 Nylon
(Unverified Data**) Zytel® PLS95G50DH2 BK261is a high flow 50% glass reinforced PA nylon resin using SHIELD Technology, only from DuPont providing exceptional Heat Resistance & High stiffness for automotive under hood.. |