Polymer Property : Tensile Stress = 3420 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 23.6 MPa

@Strain 14.67 %,
Temperature 90.0 °C
3420 psi

@Strain 14.67 %,
Temperature 194 °F
ISO 527
DuPont Performance Polymers Delrin® 100T NC010 Acetal Homopolymer  (Unverified Data**)
Delrin® 100T NC010 is a toughened, high viscosity acetal homopolymer grade with high impact resistance.Information provided by DuPont Performance Polymers
Tensile Stress 23.6 MPa

@Strain 0.350 %,
Temperature -40.0 °C
3420 psi

@Strain 0.350 %,
Temperature -40.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® HR5315HFS BK591 Polybutylene Terephthalate (PBT)  (Unverified Data**)
15% Glass Reinforced Hydrolysis Resistant Polybutylene Terephthalate with Improved Processing Crastin HR5315HFS is a 15% glass fiber reinforced moderatley toughened hydrolysis resistant polybutylene..
Tensile Stress 23.6 MPa

@Strain 0.350 %,
Temperature -40.0 °C
3420 psi

@Strain 0.350 %,
Temperature -40.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® HR5315HFS NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)
15% Glass Reinforced Hydrolysis Resistant Polybutylene Terephthalate with Improved Processing Crastin HR5315HFS is a 15% glass fiber reinforced moderatley toughened hydrolysis resistant polybutylene..
Tensile Stress 23.6 MPa

@Strain 0.860 %,
Temperature -40.0 °C
3420 psi

@Strain 0.860 %,
Temperature -40.0 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 151L NC010 Nylon 612  (Unverified Data**)
Unreinforced Polyamide 612Information provided by DuPont Performance Polymers