Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 34.0 MPa @Strain 20.0 %, Temperature 23.0 °C |
4930 psi @Strain 20.0 %, Temperature 73.4 °F |
|
Solvay TECHNYL® A 205F PA66, Conditioned Description: TECHNYL ® A 205F is an unreinforced polyamide 66 for injection molding. It is available in natural color.Benefits: The product offers two main advantages: excellent filling qualities.. |
|||
Tensile Stress | 34.0 MPa @Strain 10.0 % |
4930 psi @Strain 10.0 % |
ISO 527-1/-2 |
DuPont Performance Polymers Hytrel® 8238 Polyester Elastomer TPC-ET
(Unverified Data**) 82 Shore D Standard Performance Polyester ElastomerInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 34.0 MPa @Strain 0.580 %, Temperature 150 °C |
4930 psi @Strain 0.580 %, Temperature 302 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® PLS 95G50DH2 BK261 Nylon 6
(Unverified Data**) 50% Glass Reinforced Heat Stabilized Polyamide Zytel PLS95G50DH2 BK261is a high flow 50% glass reinforced PA nylon resin using SHIELD Technology only from DuPont providing exceptional Heat Resistanc.. |