Mechanical Properties Metric English Comments
Tensile Stress 23.01 MPa

@Strain 2.60 %,
Temperature 80.0 °C
3337 psi

@Strain 2.60 %,
Temperature 176 °F
DAM; ISO 11403-1/-2
DuPont Performance Polymers Zytel® FR7026V0F NC010 Nylon 66  (Unverified Data**)
Zytel® FR7026V0F NC010 is a flame retardant, heat stabilized, polyamide 66 resin for injection molding. It does not contain elemental phosphorous, halogens or heavy metals.Information provided by D..
Tensile Stress 23.01 MPa

@Strain 1.20 %,
Temperature 60.0 °C
3337 psi

@Strain 1.20 %,
Temperature 140 °F
DAM; ISO 11403-1/-2
DuPont Performance Polymers Zytel® FR7026V0F NC010 Nylon 66  (Unverified Data**)
Zytel® FR7026V0F NC010 is a flame retardant, heat stabilized, polyamide 66 resin for injection molding. It does not contain elemental phosphorous, halogens or heavy metals.Information provided by D..