Polymer Property : Tensile Stress = 32.8 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 32.8 MPa

@Strain 0.670 %,
Temperature 120 °C
4760 psi

@Strain 0.670 %,
Temperature 248 °F
ISO 527
DuPont Performance Polymers Crastin® SK608 BK509 PBT  (Unverified Data**)
Crastin® SK608 BK509 is a 45% glass fiber reinforced, lubricated, black polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers
Tensile Stress 32.8 MPa

@Strain 0.500 %,
Temperature -40.0 °C
4760 psi

@Strain 0.500 %,
Temperature -40.0 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 70G13L NC010 Nylon 66  (Unverified Data**)
13% Glass Reinforced Polyamide 66Zytel 70G13L NC010 is a 13% glass fiber reinforced polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers