Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 215 MPa @Strain 3.00 %, Temperature -30.0 °C |
31200 psi @Strain 3.00 %, Temperature -22.0 °F |
|
Solvay TECHNYL® A 218 V30 BK 34 NG PA66, 30% glass fiber, DRY Description: TECHNYL® A 218 V30 Black 34 NG is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. The product is available in black color.Benefits: This p.. |