Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 30.63 MPa @Strain 0.800 %, Temperature 180 °C |
4443 psi @Strain 0.800 %, Temperature 356 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN 53G60LRHF BK083 Polyphthalamide (PPA)
(Unverified Data**) 60% Glass Reinforced High Performance Polyamide with High Stiffness and Improved Flow Zytel HTN53G60LRHF BK083 is a 60% glass reinforced lubricated high performance polyamide resin with improved flo.. |
|||
Tensile Stress | 30.63 MPa @Strain 0.860 %, Temperature 90.0 °C |
4443 psi @Strain 0.860 %, Temperature 194 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® RS 30G30L NC010 Nylon 610 30% Glass Reinforced Renewably Sourced Polyamide 610 Developed for Extrusion Zytel RS 30G30L NC010 is a lubricated 30% glass fiber reinforced polyamide 610 resin containing a minimum of 40% renewabl.. |