Mechanical Properties Metric English Comments
Tensile Stress 3.04 MPa

@Strain 300 %
441 psi

@Strain 300 %
ASTM D412
Polymax® Maxelast® P3670 TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
Tensile Stress 3.04 MPa

@Strain 0.880 %,
Temperature 150 °C
441 psi

@Strain 0.880 %,
Temperature 302 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 444AHS BK152 Nylon 66  (Unverified Data**)
Toughened Heat Stabilized Polyamide 66 Zytel 444AHS is a toughened heat stabilized black polyamide 66 resin for injection molding. It is a high flow processing friendly material.Information provided..