Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 0.190 MPa @Strain 300 % |
27.6 psi @Strain 300 % |
ASTM D412 |
Polymax® Maxelast® C4803 TPE, Transparent Characteristics:Excellent clarityOvermold adhesion to polypropyleneUltrasoft TPEs with gel-like propertiesSoft and cushioning comfortSuperior colorabilityPVC, silicone, and latex freeTypical Applica.. |