Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 17.3 MPa @Strain 0.900 %, Temperature 150 °C |
2510 psi @Strain 0.900 %, Temperature 302 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Minlon® 22C NC010 Nylon 66
(Unverified Data**) 38% Mineral/Glass Reinforced Polyamide 66 Minlon 22C NC010 is a 38% mineral/glass reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Performance Polym.. |
|||
Tensile Stress | 17.3 MPa @Strain 0.140 %, Temperature -20.0 °C |
2510 psi @Strain 0.140 %, Temperature -4.00 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN FE350064 BK544 Polyphthalamide (PPA)
(Unverified Data**) Carbon Fiber Reinforced Toughened PPA High Performance Polyamide Zytel HTNFE350064 BK544 is a carbon fiber reinforced toughened heat stabilized conductive high performance polyamide resin developed .. |