Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 1.72 MPa @Strain 25.0 % |
250 psi @Strain 25.0 % |
ASTM D412 Method A |
Seals Eastern 7346 Extreme Low Temperature Service Rubber HNBR for cold temp (-50°C) and/or aqueous serviceInformation provided by Seals Eastern. |