Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Stress = 1.72 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 1.72 MPa

@Strain 300 %
249 psi

@Strain 300 %
ASTM D412
Polymax® Maxelast® P1760 TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
Tensile Stress 1.72 MPa

@Strain 100 %,
Temperature 23.0 °C
249 psi

@Strain 100 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Dynaflex™ G7950-1 NSFG Thermoplastic Elastomer (TPE)
Dynaflex™ G7950-1 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. -NSF 51 approved -FDA (see Notes) -Overmold Adhesion to Polypropylene -Soft Touch,..
Tensile Stress 1.72 MPa

@Strain 100 %,
Temperature 23.0 °C
249 psi

@Strain 100 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Dynaflex™ G7950-1001-00 Thermoplastic Elastomer (TPE)
Dynaflex™ G7950-1001-00 is an easy processing, general purpose material designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypro..
Tensile Stress 1.72 MPa

@Strain 100 %,
Temperature 23.0 °C
249 psi

@Strain 100 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Dynaflex™ G7950-9 NSFG Thermoplastic Elastomer (TPE)
Dynaflex™ G7950-9 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. -NSF 51 approved -FDA (see Notes) -Overmold Adhesion to Polypropylene -Soft Touch,..
Tensile Stress 1.72 MPa

@Strain 100 %,
Temperature 23.0 °C
249 psi

@Strain 100 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Dynaflex™ G7950-9001-02 Thermoplastic Elastomer (TPE)
Dynaflex™ G7950-9001-02 is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropylen..
Tensile Stress 1.72 MPa

@Strain 50.0 %
249 psi

@Strain 50.0 %
Average; ASTM D412 Method A
Seals Eastern 5753 Fluorocarbon-Elastomer
Features:MIL-SpecFKM general serviceInformation provided by Seals Eastern.
Tensile Stress 1.72 MPa

@Strain 25.0 %
250 psi

@Strain 25.0 %
ASTM D412 Method A
Seals Eastern 7346 Extreme Low Temperature Service Rubber
HNBR for cold temp (-50°C) and/or aqueous serviceInformation provided by Seals Eastern.
Tensile Stress 1.72 MPa

@Strain 1.02 %,
Temperature 150 °C
249 psi

@Strain 1.02 %,
Temperature 302 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® RS LC1010 NC010 Nylon 1010  (Unverified Data**)
Unreinforced Renewably Sourced Polyamide 1010 Developed for Extrusion Zytel RS LC1000 BK385 is a renewable sourced Polyamide 1010 containing a minimum of 90% renewably sourced ingredient by weight. ..
Copyright © lookpolymers.com All Rights Reserved