Mechanical Properties Metric English Comments
Tensile Stress 25.73 MPa

@Strain 17.16 %,
Temperature 90.0 °C
3732 psi

@Strain 17.16 %,
Temperature 194 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® RS 3061HSL BK039A Nylon 610  (Unverified Data**)
Unreinforced Renewably Sourced Polyamide 610 Developed for Injection Molding Zytel RS 3061HSL BK039A is a renewably sourced polyamide 610 resin containing a minimum of 60% renewably sourced ingredie..