Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 16.76 MPa @Strain 0.250 %, Temperature 120 °C |
2431 psi @Strain 0.250 %, Temperature 248 °F |
ISO 527 |
DuPont Performance Polymers Crastin® SK609 NC010 PBT
(Unverified Data**) Crastin® SK609 NC010 is a 50% glass fiber reinforced, lubricated polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 16.76 MPa @Strain 1.60 %, Temperature 80.0 °C |
2431 psi @Strain 1.60 %, Temperature 176 °F |
DAM; ISO 11403-1/-2 |
DuPont Performance Polymers Zytel® FR7026V0F NC010 Nylon 66
(Unverified Data**) Zytel® FR7026V0F NC010 is a flame retardant, heat stabilized, polyamide 66 resin for injection molding. It does not contain elemental phosphorous, halogens or heavy metals.Information provided by D.. |