Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Stress = 2360 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 16.3 MPa

@Strain 0.400 %,
Temperature -40.0 °C
2360 psi

@Strain 0.400 %,
Temperature -40.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 311DP BK402 Acetal (POM)  (Unverified Data**)
Nucleated Medium-high Viscosity Acetal Homopolymer Delrin 311DP BK402 is a medium high viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding(reduced..
Tensile Stress 16.3 MPa

@Strain 0.500 %,
Temperature 23.0 °C
2360 psi

@Strain 0.500 %,
Temperature 73.4 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 500AL NC010 Acetal (POM)  (Unverified Data**)
Lubricated Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Delrin 500AL is a medium viscosity acetal homopolymer with an advanced system of lubrication for applications requiring ..
Tensile Stress 16.27 MPa

@Strain 1.10 %,
Temperature 80.0 °C
2360 psi

@Strain 1.10 %,
Temperature 176 °F
ISO 11403-1/-2
DuPont Performance Polymers Delrin® 511P BK402 Acetal Homopolymer
Delrin® 511P is a medium viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding(reduced warpage, less shrinkage, fewer voids).Information provided ..
Tensile Stress 16.3 MPa

@Strain 0.500 %,
Temperature 23.0 °C
2360 psi

@Strain 0.500 %,
Temperature 73.4 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® FG500AL NC010 Acetal (POM)  (Unverified Data**)
Lubricated Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Developed for Food Contact Applications Delrin FG500AL is a medium viscosity acetal homopolymer lubricated for low wear ..
Tensile Stress 16.27 MPa

@Strain 0.230 %,
Temperature 180 °C
2360 psi

@Strain 0.230 %,
Temperature 356 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 70G50HSLA BK039B Nylon 66  (Unverified Data**)
50% Glass Reinforced Heat Stabilized Polyamide 66 Information provided by DuPont Performance Polymers
Tensile Stress 16.3 MPa

@Strain 0.250 %,
Temperature -20.0 °C
2360 psi

@Strain 0.250 %,
Temperature -4.00 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® SK641FR NC010 Polybutylene Terephthalate (PBT)
10% Glass Reinforced Flame Retardant Polybutylene Terephthalate Information provided by DuPont Performance Polymers
Tensile Stress 16.27 MPa

@Strain 0.800 %,
Temperature 23.0 °C
2360 psi

@Strain 0.800 %,
Temperature 73.4 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® ST830FRUV NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)
Unreinforced Flame Retardant UV Stabilized Polybutylene Terephthalate Crastin ST830FRUV NC010 is an unreinforced Super Tough flame retardant polybutylene terephthalate resin for injection molding. I..
Tensile Stress 16.3 MPa

@Strain 3.83 %,
Temperature 90.0 °C
2360 psi

@Strain 3.83 %,
Temperature 194 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 103HSL NC010 Nylon 66  (Unverified Data**)
Unreinforced Heat Stabilized Polyamide 66 Zytel 103HSL NC010 is a heat stabilized lubricated polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Tensile Stress 16.3 MPa

@Strain 1.06 %,
Temperature 120 °C
2360 psi

@Strain 1.06 %,
Temperature 248 °F
DAM; ISO 11403-1/-2
DuPont Performance Polymers Crastin® HR5315HF NC010 PBT  (Unverified Data**)
Crastin® HR5315HF is a 15% glass reinforced PBT with high flow (HF), moderately toughened, hydrolysis resistant (HR) resin. Excellent balance of properties between terminal pullout and impact resis..