Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 162 MPa @Strain 2.24 %, Temperature 40.0 °C |
23500 psi @Strain 2.24 %, Temperature 104 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Rynite® 545 NC010 Polyethylene Terephthalate (PET)
(Unverified Data**) 45% Glass Reinforced Polyethylene Terephthalate Rynite 545 NC010 is a 45% glass reinforced modified polyethylene terephthalate with greater strength and stiffness excellent dimensional stability and.. |