Mechanical Properties Metric English Comments
Tensile Stress 23.5 MPa

@Strain 0.250 %,
Temperature 0.000 °C
3410 psi

@Strain 0.250 %,
Temperature 32.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® SK643FR NC010 Polybutylene Terephthalate (PBT)
20% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin SK643FR is a flame retardant 20% glass reinforced polybutylene terephthalate molding resin. It is recognized as UL94V-0 at 0.8..
Tensile Stress 23.5 MPa

@Strain 10.0 %,
Temperature 120 °C
3410 psi

@Strain 10.0 %,
Temperature 248 °F
DAM; ISO 527
DuPont Performance Polymers Zytel® E42A NC010 Nylon 66  (Unverified Data**)
Zytel® E42A is a high viscosity polyamide 66 for injection molding and extrusion. It has improved break resistance for thick-walled parts.Information provided by DuPont Performance Polymers
Tensile Stress 23.5 MPa

@Strain 0.210 %,
Temperature 23.0 °C
3410 psi

@Strain 0.210 %,
Temperature 73.4 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® HTN 92G35DH2 BK083 Polyphthalamide (PPA)  (Unverified Data**)
35% Glass Reinforced PPA High Performance Polyamide with DuPont Zytel HTN92G35DH2 BK083 is a 35% glass reinforced high performance polyamide resin using DuPont SHIELD Technology with high flow and e..
Tensile Stress 23.5 MPa

@Strain 0.960 %,
Temperature 120 °C
3410 psi

@Strain 0.960 %,
Temperature 248 °F
ISO 527
DuPont Performance Polymers Rynite® 408 NC010 PET
Rynite® 408 NC010 is a 30% glass reinforced modified polyethylene terephthalate with improved impact resistance. Excellent balance of strength, stiffness, toughness, and temperature resistance.Inf..
Tensile Stress 23.5 MPa

@Strain 0.230 %,
Temperature 0.000 °C
3410 psi

@Strain 0.230 %,
Temperature 32.0 °F
ISO 527
DuPont Performance Polymers Rynite® 408 NC010 PET
Rynite® 408 NC010 is a 30% glass reinforced modified polyethylene terephthalate with improved impact resistance. Excellent balance of strength, stiffness, toughness, and temperature resistance.Inf..