Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 23.5 MPa @Strain 0.250 %, Temperature 0.000 °C |
3410 psi @Strain 0.250 %, Temperature 32.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® SK643FR NC010 Polybutylene Terephthalate (PBT) 20% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin SK643FR is a flame retardant 20% glass reinforced polybutylene terephthalate molding resin. It is recognized as UL94V-0 at 0.8.. |
|||
Tensile Stress | 23.5 MPa @Strain 10.0 %, Temperature 120 °C |
3410 psi @Strain 10.0 %, Temperature 248 °F |
DAM; ISO 527 |
DuPont Performance Polymers Zytel® E42A NC010 Nylon 66
(Unverified Data**) Zytel® E42A is a high viscosity polyamide 66 for injection molding and extrusion. It has improved break resistance for thick-walled parts.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 23.5 MPa @Strain 0.210 %, Temperature 23.0 °C |
3410 psi @Strain 0.210 %, Temperature 73.4 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN 92G35DH2 BK083 Polyphthalamide (PPA)
(Unverified Data**) 35% Glass Reinforced PPA High Performance Polyamide with DuPont Zytel HTN92G35DH2 BK083 is a 35% glass reinforced high performance polyamide resin using DuPont SHIELD Technology with high flow and e.. |
|||
Tensile Stress | 23.5 MPa @Strain 0.960 %, Temperature 120 °C |
3410 psi @Strain 0.960 %, Temperature 248 °F |
ISO 527 |
DuPont Performance Polymers Rynite® 408 NC010 PET Rynite® 408 NC010 is a 30% glass reinforced modified polyethylene terephthalate with improved impact resistance. Excellent balance of strength, stiffness, toughness, and temperature resistance.Inf.. |
|||
Tensile Stress | 23.5 MPa @Strain 0.230 %, Temperature 0.000 °C |
3410 psi @Strain 0.230 %, Temperature 32.0 °F |
ISO 527 |
DuPont Performance Polymers Rynite® 408 NC010 PET Rynite® 408 NC010 is a 30% glass reinforced modified polyethylene terephthalate with improved impact resistance. Excellent balance of strength, stiffness, toughness, and temperature resistance.Inf.. |