Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 14.67 MPa @Strain 18.87 %, Temperature 150 °C |
2128 psi @Strain 18.87 %, Temperature 302 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® RS 3061HSL BK039A Nylon 610
(Unverified Data**) Unreinforced Renewably Sourced Polyamide 610 Developed for Injection Molding Zytel RS 3061HSL BK039A is a renewably sourced polyamide 610 resin containing a minimum of 60% renewably sourced ingredie.. |