Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 145 MPa @Strain 2.00 % |
21000 psi @Strain 2.00 % |
|
Solvay TECHNYLSTARâ„¢ AFX 218 V50 PA6, 50% glass filled, DRY Description TECHNYLSTARâ„¢ AFX 218 V50 is based on a patented high flow polyamide 66 resin (Technylstar), heat stabilized, reinforced with 50% of glass fiber, for injection molding. It is availab.. |
|||
Tensile Stress | 145 MPa @Strain 2.00 % |
21000 psi @Strain 2.00 % |
|
Solvay TECHNYLSTARâ„¢ S 218 V30 PA6, 30% glass filled, DRY Description: TECHNYLSTARâ„¢ S 218 V30 is based on a patented high flow polyamide 6 resin (TechnylStar), heat stabilized, reinforced with 30% of glass fiber, for injection molding. This product is.. |
|||
Tensile Stress | 145 MPa @Strain 0.100 % |
21000 psi @Strain 0.100 % |
Process Temperature T1 |
COI Ceramics Sylramic™ S300 Silicon Carbide Ceramic Matrix Composite, SiC Description: Engineered ceramic composite structures for a broad range of industries and applications.Reinforcing Fiber Flexibility: S300 - Sylramic SiC Preceramic Polymer Matrix Precursors: S300 - .. |
|||
Tensile Stress | 145 MPa @Strain 8.00 %, Temperature 120 °C |
21000 psi @Strain 8.00 %, Temperature 248 °F |
|
Akro-Plastic Akroloy® PA GF 50 (2706) PA 6.6 & PA6I/6T Dry, 50% Glass Filled One of the most characteristic properties of polyamide (PA 6.6) is the absorption of moisture. This essentially leads to increased toughness and elongation at break, to name the most important param.. |