Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 210 MPa @Strain 3.00 %, Temperature -30.0 °C |
30500 psi @Strain 3.00 %, Temperature -22.0 °F |
|
Solvay TECHNYL® A 218 V30 PA66, 30% glass fiber, DRY Description: TECHNYL® A 218 V30 is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The .. |
|||
Tensile Stress | 210 MPa @Strain 2.00 %, Temperature -40.0 °C |
30500 psi @Strain 2.00 %, Temperature -40.0 °F |
|
Solvay TECHNYL® A 218 V35 PA66, 35% glass fiber, DRY Description: TECHNYL® A 218 V35 is a polyamide 66, reinforced with 35% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The .. |
|||
Tensile Stress | 210 MPa @Strain 2.00 % |
30500 psi @Strain 2.00 % |
|
Solvay TECHNYLSTARâ„¢ SX 218 V50 PA6, 50% glass filled, DRY Description: TECHNYLSTARâ„¢ SX 218 V50 is based on a patented high flow polyamide 6 resin (Technylstar), heat stabilized, reinforced with 50% of glass fiber, for injection molding. This product i.. |