Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 207 MPa @Strain 0.300 % |
30000 psi @Strain 0.300 % |
|
COI Ceramics Nextel™ AS-N720 Oxide Ceramic Matrix Composite, Aluminosilicate Description: Oxide ceramic matrix composites products are based upon sol-gel derived matrices and 3M Corporation's Nextel™ fiber products. These materials can be used up to 1200ºC (2200ºF) in air.. |
|||
Tensile Stress | 207 MPa @Strain 0.00400 % |
30000 psi @Strain 0.00400 % |
|
COI Ceramics Sylramic™ S400 Silicon Carbide Ceramic Matrix Composite, Carbon Description: Engineered ceramic composite structures for a broad range of industries and applications.Reinforcing Fiber Flexibility: S400 - Carbon Preceramic Polymer Matrix Precursors: S400 - Crysta.. |
|||
Tensile Stress | 207 MPa @Strain 3.40 %, Temperature -20.0 °C |
30000 psi @Strain 3.40 %, Temperature -4.00 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 73G30T NC010 Nylon 6
(Unverified Data**) 30% Glass Reinforced Toughened Polyamide 6 Zytel 73G30T NC010 is a 30% glass fiber reinforced toughened polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |