Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

COI Ceramics Nextel™ AS-N720 Oxide Ceramic Matrix Composite, Aluminosilicate

Category Ceramic , Ceramic Matrix Composite , Oxide , Aluminum Oxide , Silicon Oxide
Manufacturer COI Ceramics
Trade Name Nextel™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF COI Ceramics Nextel™ AS-N720 Oxide Ceramic Matrix Composite, Aluminosilicate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Oxide ceramic matrix composites products are based upon sol-gel derived matrices and 3M Corporation's Nextel™ fiber products. These materials can be used up to 1200ºC (2200ºF) in air environments and are primarily used in both Aerospace and Gas Turbine applications.Ceramic Matrix System: Water Based Sol-Gel Processing, Versatile Matrix ChemistryTypical Applications for Oxide CMCs: Rotocraft Exhaust Systems, Advanced Thermal, Advanced CombustorHighest Temperature & Creep PerformanceInformation from COI Ceramics, Inc.
Physical Properties Metric English Comments
Density 2.60 g/cc
0.0939 lb/in³
Porosity 25 %
25 %
Mechanical Properties Metric English Comments
Tensile Strength 220 MPa
31900 psi
Tensile Stress 89.6 MPa

@Strain 0.100 %
13000 psi

@Strain 0.100 %
152 MPa

@Strain 0.200 %
22000 psi

@Strain 0.200 %
207 MPa

@Strain 0.300 %
30000 psi

@Strain 0.300 %
Tensile Modulus 76.0 GPa
11000 ksi
Shear Strength 14.3 MPa
2070 psi
Short Beam
Thermal Properties Metric English Comments
CTE, linear 6.30 µm/m-°C
3.50 µin/in-°F
Maximum Service Temperature, Air 1100 °C
2010 °F
Descriptive Properties Value Comments
Nominal Fiber Volume (%) 45