Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 1.38 MPa @Strain 300 %, Temperature 23.0 °C |
200 psi @Strain 300 %, Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Versaflex™ CL30 Thermoplastic Elastomer (TPE) Versaflex™ CL30 is an easy processing compound designed for use in injection molding and extrusion applications where water-clarity and excellent colorability are required. - Excellent Clarity - Ex.. |
|||
Tensile Stress | 1.38 MPa @Strain 100 %, Temperature 23.0 °C |
200 psi @Strain 100 %, Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Versaflex™ CL40 Thermoplastic Elastomer (TPE) Versaflex™ CL40 is an easy processing compound designed for use in injection molding applications where water-clarity and excellent colorability are required. - Excellent Clarity - Excellent Colora.. |
|||
Tensile Stress | 1.38 MPa @Strain 300 % |
200 psi @Strain 300 % |
ASTM D412 |
Polymax® Maxelast® P1745N TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Stress | 1.38 MPa @Strain 300 % |
200 psi @Strain 300 % |
ASTM D412 |
Polymax® Maxelast® P3932C TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Stress | 1.38 MPa @Strain 300 %, Temperature 23.0 °C |
200 psi @Strain 300 %, Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Dynaflex™ G7930-1001-00 Thermoplastic Elastomer (TPE) Dynaflex™ G7930-1001-00 is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Non-Slip Grip - Overmold Adhesion.. |
|||
Tensile Stress | 1.38 MPa @Strain 300 %, Temperature 23.0 °C |
200 psi @Strain 300 %, Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Dynaflex™ G7930-9 NSFG Thermoplastic Elastomer (TPE) Dynaflex™ G7930-9 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. - NSF 51 approved - FDA (see Notes) - Overmold Adhesion to Polypropylene - Soft To.. |
|||
Tensile Stress | 1.38 MPa @Strain 300 %, Temperature 23.0 °C |
200 psi @Strain 300 %, Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Dynaflex™ G7930-9001-02 Thermoplastic Elastomer (TPE) Dynaflex™ G7930-9001-02 is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Non-Slip Grip - Overmold Adhesion.. |
|||
Tensile Stress | 1.38 MPa @Strain 300 %, Temperature 23.0 °C |
200 psi @Strain 300 %, Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Dynaflex™ G7930-1 NSFG Thermoplastic Elastomer (TPE) Dynaflex™ G7930-1 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. - NSF 51 approved - FDA (see Notes) - Overmold Adhesion to Polypropylene - Soft To.. |
|||
Tensile Stress | 1.38 MPa @Strain 100 % |
200 psi @Strain 100 % |
ASTM D412 |
Teknor Apex Telcar® TL-1522B Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Tensile Stress | 1.38 MPa @Strain 0.000 %, Temperature 60.0 °C |
200 psi @Strain 0.000 %, Temperature 140 °F |
DAM; ISO 11403-1/-2 |
DuPont Performance Polymers Zytel® PLUS PLS93G35DH1 BK261 Nylon 6
(Unverified Data**) Zytel® PLS93G35DH1 BK261 is a 35% glass reinforced PA6 using SHIELD Technology, only from DuPont, it provides exceptional welding resistance & retention over time thanks to excellent Heat Resistanc.. |
|||
Tensile Stress | 1.38 MPa @Strain 0.000 %, Temperature 150 °C |
200 psi @Strain 0.000 %, Temperature 302 °F |
DAM; ISO 11403-1/-2 |
DuPont Performance Polymers Zytel® PLUS PLS95G50DH2 BK261 Nylon
(Unverified Data**) Zytel® PLS95G50DH2 BK261is a high flow 50% glass reinforced PA nylon resin using SHIELD Technology, only from DuPont providing exceptional Heat Resistance & High stiffness for automotive under hood.. |