Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 2.76 MPa @Strain 100 % |
400 psi @Strain 100 % |
ASTM D412 |
Polymax® Maxelast® A9870 TPE, ABS/PC Overmold Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesInform.. |
|||
Tensile Stress | 2.76 MPa @Strain 300 % |
400 psi @Strain 300 % |
ASTM D412 |
Polymax® Maxelast® P1855 TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Stress | 2.76 MPa @Strain 300 %, Temperature 23.0 °C |
400 psi @Strain 300 %, Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Dynaflex™ G2709-1000-00 Thermoplastic Elastomer (TPE) Dynaflex™ G2709-1000-00 is an easy processing TPE designed for injection molding and extrusion applications that require FDA compliance. - Excellent Colorability - Good Ozone/UV Stability - Overmol.. |
|||
Tensile Stress | 2.76 MPa @Strain 300 %, Temperature 23.0 °C |
400 psi @Strain 300 %, Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Dynaflex™ G7650-9 (Black) Thermoplastic Elastomer (TPE) Dynaflex™ G7650-9 (Black) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropyl.. |
|||
Tensile Stress | 2.76 MPa @Strain 100 % |
400 psi @Strain 100 % |
ASTM D412 |
Teknor Apex Telcar® TL-1336 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Tensile Stress | 2.76 MPa @Strain 0.0400 %, Temperature -20.0 °C |
400 psi @Strain 0.0400 %, Temperature -4.00 °F |
50%RH; ISO 11403-1/-2 |
DuPont Performance Polymers Zytel® PLUS PLS93G35DH1 BK261 Nylon 6
(Unverified Data**) Zytel® PLS93G35DH1 BK261 is a 35% glass reinforced PA6 using SHIELD Technology, only from DuPont, it provides exceptional welding resistance & retention over time thanks to excellent Heat Resistanc.. |