Polymer Property : Tensile Stress = 2.48 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 2.48 MPa

@Strain 300 %,
Temperature 23.0 °C
360 psi

@Strain 300 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Versaflex™ CL2250 Thermoplastic Elastomer (TPE)
Versaflex™ CL2250 is an easy processing compound designed for use in injection molding applications where FDA compliance, clarity and enhanced heat resistance are required. - Excellent Clarity - Ov..
Tensile Stress 2.48 MPa

@Strain 100 %,
Temperature 21.0 °C
360 psi

@Strain 100 %,
Temperature 69.8 °F
Die C2 hr; ASTM D412
PolyOne Versalloy™ XL 9070-1 Thermoplastic Elastomer (TPE)
Versalloy™ XL 9070-1 is a TPV alloy with exceptional flow properties and surface aesthetics for a variety of applications. - Excellent Flow for Long, Thin Flow Paths - Exceptional Colorability - Ov..
Tensile Stress 2.48 MPa

@Strain 100 %,
Temperature 23.0 °C
360 psi

@Strain 100 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Versalloy™ XL 9070X-9 Thermoplastic Elastomer (TPE)
Versalloy™ XL 9070X-9 is a TPV alloy with exceptional flow properties and surface aesthetics for a variety of applications. - Exceptional Flow for Long, Thin Flow Paths - Overmold Adhesion to Polyp..
Tensile Stress 2.48 MPa

@Strain 100 %,
Temperature 23.0 °C
360 psi

@Strain 100 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Dynaflex™ G7430-9001-00 Thermoplastic Elastomer (TPE)
Dynaflex™ G7430-9001-00 is an easy processing, high performance compound designed for use in applications requiring tough, durable material. - Excellent Heat Stability - Good Ozone and UV Stability..
Tensile Stress 2.48 MPa

@Strain 300 %,
Temperature 23.0 °C
360 psi

@Strain 300 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Dynaflex™ G7640-9 (Black) Thermoplastic Elastomer (TPE)
Dynaflex™ G7640-9 (Black) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropyl..
Tensile Stress 2.48 MPa

@Strain 300 %,
Temperature 23.0 °C
360 psi

@Strain 300 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Dynaflex™ G7950-1 NSFG Thermoplastic Elastomer (TPE)
Dynaflex™ G7950-1 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. -NSF 51 approved -FDA (see Notes) -Overmold Adhesion to Polypropylene -Soft Touch,..
Tensile Stress 2.48 MPa

@Strain 300 %,
Temperature 23.0 °C
360 psi

@Strain 300 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Dynaflex™ G7950-1001-00 Thermoplastic Elastomer (TPE)
Dynaflex™ G7950-1001-00 is an easy processing, general purpose material designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypro..
Tensile Stress 2.48 MPa

@Strain 300 %,
Temperature 23.0 °C
360 psi

@Strain 300 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Dynaflex™ G7950-9 NSFG Thermoplastic Elastomer (TPE)
Dynaflex™ G7950-9 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. -NSF 51 approved -FDA (see Notes) -Overmold Adhesion to Polypropylene -Soft Touch,..
Tensile Stress 2.48 MPa

@Strain 300 %,
Temperature 23.0 °C
360 psi

@Strain 300 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Dynaflex™ G7950-9001-02 Thermoplastic Elastomer (TPE)
Dynaflex™ G7950-9001-02 is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropylen..
Tensile Stress 2.48 MPa

@Strain 300 %,
Temperature 23.0 °C
360 psi

@Strain 300 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Dynaflex™ G7640-1 (Natural) Thermoplastic Elastomer (TPE)
Dynaflex™ G7640-1 (Natural) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Non-Slip Grip - Overmold Adhe..
Tensile Stress >= 2.48 MPa

@Strain 50.0 %
>= 360 psi

@Strain 50.0 %
ASTM D412 Method A
Seals Eastern 5794 Fluorocarbon-Elastomer