Polymer Property : Tensile Stress = 2.29 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 2.29 MPa

@Strain 19.58 %,
Temperature 120 °C
332 psi

@Strain 19.58 %,
Temperature 248 °F
ISO 527
DuPont Performance Polymers Hytrel® G4078W TPC-ET  (Unverified Data**)
Hytrel® G4078W is a low modulus grade with nominal hardness of 40D. It contains non-discoloring stabilizer. It can be processed by many conventional thermoplastic processing techniques like inject..