Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 2.17 MPa @Strain 0.000 %, Temperature 60.0 °C |
315 psi @Strain 0.000 %, Temperature 140 °F |
DAM; ISO 11403-1/-2 |
DuPont Performance Polymers Zytel® PLUS PLS95G50DH2 BK261 Nylon
(Unverified Data**) Zytel® PLS95G50DH2 BK261is a high flow 50% glass reinforced PA nylon resin using SHIELD Technology, only from DuPont providing exceptional Heat Resistance & High stiffness for automotive under hood.. |