Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 13.32 MPa @Strain 3.00 %, Temperature 90.0 °C |
1932 psi @Strain 3.00 %, Temperature 194 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 153HSL NC010 Nylon 612
(Unverified Data**) Unreinforced Heat Stabilized Polyamide 612 Information provided by DuPont Performance Polymers |