Tensile Stress 131.91 MPa

@Strain 1.12 %,
Temperature -40.0 °C
19132 psi

@Strain 1.12 %,
Temperature -40.0 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® RS 32CG20HSL BK409 Nylon 610  (Unverified Data**)
20% Carbon/Glass Reinforced Renewably Sourced Polyamide 610 Information provided by DuPont Performance Polymers