Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 19.98 MPa @Strain 1.85 %, Temperature 40.0 °C |
2898 psi @Strain 1.85 %, Temperature 104 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® S600F10 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l Unreinforced High Viscosity Polybutylene Terephthalate Developed for Extrusion and Injection Molding Crastin S600F10 NC010 is an unreinforced lubricated medium high viscosity polybutylene terephthal.. |
|||
Tensile Stress | 19.98 MPa @Strain 0.240 %, Temperature 40.0 °C |
2898 psi @Strain 0.240 %, Temperature 104 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® RS 32CG20HSL BK409 Nylon 610
(Unverified Data**) 20% Carbon/Glass Reinforced Renewably Sourced Polyamide 610 Information provided by DuPont Performance Polymers |