Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 19.82 MPa @Strain 14.51 %, Temperature 90.0 °C |
2875 psi @Strain 14.51 %, Temperature 194 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® RS LC1000 BK385 Nylon 1010 UV Stabilized Renewably Sourced Polyamide 1010 Developed for Extrusion Zytel RS LC1000 BK385 is a renewable sourced Polyamide 1010 containing a minimum of 90% renewably sourced ingredient by weight... |