Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 12.72 MPa @Strain 0.600 %, Temperature 60.0 °C |
1845 psi @Strain 0.600 %, Temperature 140 °F |
DAM; ISO 11403-1/-2 |
DuPont Performance Polymers Zytel® FR7026V0F NC010 Nylon 66
(Unverified Data**) Zytel® FR7026V0F NC010 is a flame retardant, heat stabilized, polyamide 66 resin for injection molding. It does not contain elemental phosphorous, halogens or heavy metals.Information provided by D.. |