Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 18.98 MPa @Strain 2.70 %, Temperature 150 °C |
2753 psi @Strain 2.70 %, Temperature 302 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Minlon® 10B40 NC010 Nylon 66
(Unverified Data**) 40% Mineral Reinforced Polyamide 66Minlon 10B40 NC010 is a 40% mineral reinforced polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |