Polymer Property : Tensile Stress = 17700 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 122 MPa

@Strain 2.00 %,
Temperature 60.0 °C
17700 psi

@Strain 2.00 %,
Temperature 140 °F
Solvay TECHNYL® A 218 V35 PA66, 35% glass fiber, DRY
Description: TECHNYL® A 218 V35 is a polyamide 66, reinforced with 35% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The ..
Tensile Stress 122 MPa

@Strain 2.00 %,
Temperature 23.0 °C
17700 psi

@Strain 2.00 %,
Temperature 73.4 °F
Solvay TECHNYL® A 60 G1 V25 PA66, 25% glass fiber, DRY
Description: TECHNYL® A 60G1 V25 is a 25% GF reinforced organophosphorous flame retarded grade based on a patented high flow polyamide 66 resin. This product is heat stabilized and provides optim..
Tensile Stress 122 MPa

@Strain 1.50 %,
Temperature 23.0 °C
17700 psi

@Strain 1.50 %,
Temperature 73.4 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® SK605 NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)
30% Glass Reinforced Polybutylene Terephthalate Crastin SK605 NC010 is a 30% glass fiber reinforced lubricated polybutylene terephthalate resin for injection molding.Information provided by DuPont P..
Tensile Stress 122 MPa

@Strain 1.36 %,
Temperature -20.0 °C
17700 psi

@Strain 1.36 %,
Temperature -4.00 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 73G30T NC010 Nylon 6  (Unverified Data**)
30% Glass Reinforced Toughened Polyamide 6 Zytel 73G30T NC010 is a 30% glass fiber reinforced toughened polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers
Tensile Stress 122 MPa

@Strain 1.10 %,
Temperature 90.0 °C
17700 psi

@Strain 1.10 %,
Temperature 194 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® HTN 51G45HSL NC010 Polyphthalamide (PPA)  (Unverified Data**)
45% Glass Reinforced PPA High Performance Polyamide Zytel HTN51G45HSL NC010 is a 45% glass reinforced heat stabilized lubricated high performance polyamide resin. It is also a PPA resin.Information ..