Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 12.05 MPa @Strain 0.490 %, Temperature 23.0 °C |
1748 psi @Strain 0.490 %, Temperature 73.4 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 153HSL NC010 Nylon 612
(Unverified Data**) Unreinforced Heat Stabilized Polyamide 612 Information provided by DuPont Performance Polymers |