Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 119.26 MPa @Strain 1.78 %, Temperature 40.0 °C |
17297 psi @Strain 1.78 %, Temperature 104 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 70G50HSLA BK039B Nylon 66
(Unverified Data**) 50% Glass Reinforced Heat Stabilized Polyamide 66 Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 119.26 MPa @Strain 2.35 %, Temperature -20.0 °C |
17297 psi @Strain 2.35 %, Temperature -4.00 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 73G15L NC010 Nylon 6
(Unverified Data**) 15% Glass Reinforced Polyamide 6Zytel 73G15L NC010 is a 15% glass fiber reinforced polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |