Mechanical Properties Metric English Comments
Tensile Stress 160.7 MPa

@Strain 3.20 %,
Temperature -40.0 °C
23310 psi

@Strain 3.20 %,
Temperature -40.0 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Minlon® 22C NC010 Nylon 66  (Unverified Data**)
38% Mineral/Glass Reinforced Polyamide 66 Minlon 22C NC010 is a 38% mineral/glass reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Performance Polym..