Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 160 MPa @Strain 2.00 %, Temperature 23.0 °C |
23200 psi @Strain 2.00 %, Temperature 73.4 °F |
|
Solvay TECHNYL® A 218 V30 PA66, 30% glass fiber, DRY Description: TECHNYL® A 218 V30 is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The .. |
|||
Tensile Stress | 160 MPa @Strain 2.00 %, Temperature 0.000 °C |
23200 psi @Strain 2.00 %, Temperature 32.0 °F |
|
Solvay TECHNYL® A 218 V35 PA66, 35% glass fiber, Conditioned Description: TECHNYL® A 218 V35 is a polyamide 66, reinforced with 35% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The .. |
|||
Tensile Stress | 160 MPa @Strain 2.00 % |
23200 psi @Strain 2.00 % |
|
Solvay TECHNYL® C 218 V 30 PA6, 30% glass fiber, DRY Description: TECHNYL® C 218 V30 is a polyamide 6, heat stabilized, reinforced with 30% of glass fiber, for injection molding. This product is available in black color.Benefits: The product offers.. |
|||
Tensile Stress | 160 MPa @Strain 0.300 %, Temperature 25.0 °C |
23200 psi @Strain 0.300 %, Temperature 77.0 °F |
|
COI Ceramics Nextel™ A-N720 Oxide Ceramic Matrix Composite, Alumina Description: Oxide ceramic matrix composites products are based upon sol-gel derived matrices and 3M Corporation's Nextel™ fiber products. These materials can be used up to 1200ºC (2200ºF) in air.. |
|||
Tensile Stress | 160 MPa @Strain 0.300 %, Temperature 1200 °C |
23200 psi @Strain 0.300 %, Temperature 2190 °F |
|
COI Ceramics Nextel™ A-N720 Oxide Ceramic Matrix Composite, Alumina Description: Oxide ceramic matrix composites products are based upon sol-gel derived matrices and 3M Corporation's Nextel™ fiber products. These materials can be used up to 1200ºC (2200ºF) in air.. |
|||
Tensile Stress | 160 MPa @Strain 0.300 %, Temperature 1204 °C |
23200 psi @Strain 0.300 %, Temperature 2199 °F |
|
COI Ceramics Sylramic™ S200 Silicon Carbide Ceramic Matrix Composite, CG Nicalon Engineered ceramic composite structure.Reinforcing Fiber Flexibility: S400 - Carbon Preceramic Polymer Matrix Precursors: S400 - Crystalline (SiC + Si3N4) or SiCPhysical Attributes: Dense Matrix ( |
|||
Tensile Stress | 160 MPa @Strain 1.00 %, Temperature 23.0 °C |
23200 psi @Strain 1.00 %, Temperature 73.4 °F |
|
Akro-Plastic Akroloy® PA GF 50 (2706) PA 6.6 & PA6I/6T Dry, 50% Glass Filled One of the most characteristic properties of polyamide (PA 6.6) is the absorption of moisture. This essentially leads to increased toughness and elongation at break, to name the most important param.. |
|||
Tensile Stress | 160 MPa @Strain 2.00 %, Temperature 120 °C |
23200 psi @Strain 2.00 %, Temperature 248 °F |
|
Akro-Plastic Akromid® T1 GF 50 (3101) PPA Dry, 50% Glass Filled The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high.. |