Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 108 MPa @Strain 1.50 %, Temperature -20.0 °C |
15700 psi @Strain 1.50 %, Temperature -4.00 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® SK643FR NC010 Polybutylene Terephthalate (PBT) 20% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin SK643FR is a flame retardant 20% glass reinforced polybutylene terephthalate molding resin. It is recognized as UL94V-0 at 0.8.. |
|||
Tensile Stress | 108 MPa @Strain 2.00 %, Temperature -40.0 °C |
15700 psi @Strain 2.00 %, Temperature -40.0 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Minlon® 73M40 NC010 Nylon 6
(Unverified Data**) 40% Mineral Reinforced Polyamide 6 Minlon 73M40 NC010 is a 40% mineral reinforced heat stabilized polyamide 6 resin for injection molding. It has isotropic properties and low warpage.Information pro.. |
|||
Tensile Stress | 108.25 MPa @Strain 2.89 %, Temperature 0.000 °C |
15700 psi @Strain 2.89 %, Temperature 32.0 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Minlon® 73M40 NC010 Nylon 6
(Unverified Data**) 40% Mineral Reinforced Polyamide 6 Minlon 73M40 NC010 is a 40% mineral reinforced heat stabilized polyamide 6 resin for injection molding. It has isotropic properties and low warpage.Information pro.. |
|||
Tensile Stress | 108 MPa @Strain 1.10 %, Temperature 23.0 °C |
15700 psi @Strain 1.10 %, Temperature 73.4 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Minlon® EFE6053 BK413 Nylon 66
(Unverified Data**) 40% Mineral/Glass Reinforced Polyamide 66 Minlon EFE6053 BK413 is a 40% mineral/glass reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Performance P.. |
|||
Tensile Stress | 108.25 MPa @Strain 1.10 %, Temperature 23.0 °C |
15700 psi @Strain 1.10 %, Temperature 73.4 °F |
DAM; ISO 11403-1/-2 |
DuPont Performance Polymers Zytel® 80G43HS1L BK104 Nylon 66
(Unverified Data**) Zytel® 80G43HS1L BK104 is a 43% glass fiber reinforced, heat stabilized, black polyamide 66 resin with superior impact resistance.Information provided by DuPont Performance Polymers |