Mechanical Properties Metric English Comments
Tensile Stress 157.63 MPa

@Strain 2.10 %,
Temperature -20.0 °C
22862 psi

@Strain 2.10 %,
Temperature -4.00 °F
ISO 11403-1 -2
DuPont Performance Polymers Rynite® GW520CS NC010 Polyethylene Terephthalate (PET)
20% Glass Reinforced Flame Retardant Polyethylene Terephthalate with Improved Glow Wire Performance Rynite GW520CS NC010 is a 20% glass fiber reinforced flame retardant color stabilized modified pol..