Polymer Property : Tensile Stress = 15400 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 106.2 MPa

@Strain 1.60 %,
Temperature -40.0 °C
15400 psi

@Strain 1.60 %,
Temperature -40.0 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 73G15L NC010 Nylon 6  (Unverified Data**)
15% Glass Reinforced Polyamide 6Zytel 73G15L NC010 is a 15% glass fiber reinforced polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers
Tensile Stress 106 MPa

@Strain 1.50 %,
Temperature -40.0 °C
15400 psi

@Strain 1.50 %,
Temperature -40.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® LW9020 NC010 PBT+ASA  (Unverified Data**)
20% Glass Reinforced Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9020 NC010 is a 20% glass fiber reinforced polybutylene terephthalate blend for injection molding. ..