Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 88.75 MPa @Strain 1.00 %, Temperature -40.0 °C |
12870 psi @Strain 1.00 %, Temperature -40.0 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® FR50 NC010A Nylon 66
(Unverified Data**) 25% Glass Reinforced Flame Retardant Polyamide 66 Zytel FR50 NC010A is a 25% glass fiber reinforced flame retardant polyamide 66 resin for injection molding.Information provided by DuPont Performanc.. |
|||
Tensile Stress | 88.71 MPa @Strain 4.44 %, Temperature -40.0 °C |
12870 psi @Strain 4.44 %, Temperature -40.0 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 444AHS BK152 Nylon 66
(Unverified Data**) Toughened Heat Stabilized Polyamide 66 Zytel 444AHS is a toughened heat stabilized black polyamide 66 resin for injection molding. It is a high flow processing friendly material.Information provided.. |