Mechanical Properties Metric English Comments
Tensile Stress 85.05 MPa

@Strain 4.18 %,
Temperature 40.0 °C
12340 psi

@Strain 4.18 %,
Temperature 104 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 80G33L NC010 Nylon 66  (Unverified Data**)
33% Glass Reinforced Toughened Polyamide 66 Zytel 80G33L NC010 is a 33% glass fiber reinforced polyamide 66 resin with outstanding impact resistance developed using DuPont Super Tough technology.Inf..
Tensile Stress 85.05 MPa

@Strain 4.04 %,
Temperature 90.0 °C
12340 psi

@Strain 4.04 %,
Temperature 194 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® EFE7374 BK416 Nylon 6  (Unverified Data**)
40% Glass Reinforced Toughened Polyamide 6 Zytel EFE7374 is a 40% fiber reinforced heat stabilized lubricated toughened polyamide 6 for injection molding. It has an improved impact resistance and ex..