Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 84.54 MPa @Strain 0.620 %, Temperature 23.0 °C |
12260 psi @Strain 0.620 %, Temperature 73.4 °F |
ISO 527 |
DuPont Performance Polymers Crastin® SK609 NC010 PBT
(Unverified Data**) Crastin® SK609 NC010 is a 50% glass fiber reinforced, lubricated polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 84.53 MPa @Strain 1.30 %, Temperature 23.0 °C |
12260 psi @Strain 1.30 %, Temperature 73.4 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Minlon® 22C NC010 Nylon 66
(Unverified Data**) 38% Mineral/Glass Reinforced Polyamide 66 Minlon 22C NC010 is a 38% mineral/glass reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Performance Polym.. |