Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 83.98 MPa @Strain 6.94 %, Temperature 180 °C |
12180 psi @Strain 6.94 %, Temperature 356 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® PLS 95G50DH2 BK261 Nylon 6
(Unverified Data**) 50% Glass Reinforced Heat Stabilized Polyamide Zytel PLS95G50DH2 BK261is a high flow 50% glass reinforced PA nylon resin using SHIELD Technology only from DuPont providing exceptional Heat Resistanc.. |