Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 82.82 MPa @Strain 0.900 %, Temperature -40.0 °C |
12010 psi @Strain 0.900 %, Temperature -40.0 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Minlon® 10B40 NC010 Nylon 66
(Unverified Data**) 40% Mineral Reinforced Polyamide 66Minlon 10B40 NC010 is a 40% mineral reinforced polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 82.81 MPa @Strain 2.13 %, Temperature 23.0 °C |
12010 psi @Strain 2.13 %, Temperature 73.4 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 80G33L NC010 Nylon 66
(Unverified Data**) 33% Glass Reinforced Toughened Polyamide 66 Zytel 80G33L NC010 is a 33% glass fiber reinforced polyamide 66 resin with outstanding impact resistance developed using DuPont Super Tough technology.Inf.. |