Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 119.91 MPa @Strain 3.10 %, Temperature 23.0 °C |
17392 psi @Strain 3.10 %, Temperature 73.4 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 70G13L NC010 Nylon 66
(Unverified Data**) 13% Glass Reinforced Polyamide 66Zytel 70G13L NC010 is a 13% glass fiber reinforced polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |