Mechanical Properties Metric English Comments
Tensile Stress 81.35 MPa

@Strain 1.54 %,
Temperature -20.0 °C
11800 psi

@Strain 1.54 %,
Temperature -4.00 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® HR5315HF NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)&
15% Glass Reinforced Hydrolysis Resistant Polybutylene Terephthalate Crastin HR5315HF is a 15% glass reinforced PBT with high flow (HF) moderately toughened hydrolysis resistant (HR) resin. Excellen..
Tensile Stress 81.4 MPa

@Strain 10.4 %,
Temperature -20.0 °C
11800 psi

@Strain 10.4 %,
Temperature -4.00 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 127UV NC010 Acetal (POM)  (Unverified Data**)
UV Stabilized High Viscosity Acetal HomopolymerDelrin 127UV is a high viscosity acetal homopolymer with UV stabilizers developed for automotive interior applications. It has improvements in UV aging..
Tensile Stress 81.6 MPa

@Strain 1.11 %,
Temperature 23.0 °C
11800 psi

@Strain 1.11 %,
Temperature 73.4 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 70G43L NC010 Nylon 66  (Unverified Data**)
43% Glass Reinforced Polyamide 66Zytel 70G43L NC010 is a 43% glass fiber reinforced polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Tensile Stress 81.37 MPa

@Strain 7.00 %,
Temperature 150 °C
11800 psi

@Strain 7.00 %,
Temperature 302 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 74G33W BK196 Nylon 66  (Unverified Data**)
33% Glass Reinforced UV Stabilized Polyamide 66 + Polyamide 6 Zytel 74G33W BK196 is a high gloss automotive weatherable black 33% glass reinforced nylon 66 and nylon 6 comelt resin.Information provi..
Tensile Stress 81.39 MPa

@Strain 1.06 %,
Temperature 40.0 °C
11800 psi

@Strain 1.06 %,
Temperature 104 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® HTN FR52G30NH NC010 Polyphthalamide (PPA)  (Unverified Data**)
30% Glass Reinforced Flame Retardant Non-Halogenated PPA High Performance Polyamide Zytel HTNFR52G30NH NC010 is a 30% glass reinforced flame retardant lubricated high performance polyamide resin. It..
Tensile Stress 81.1 MPa

@Strain 1.50 %,
Temperature 0.000 °C
11800 psi

@Strain 1.50 %,
Temperature 32.0 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Minlon® 11C40 NC010 Nylon 66  (Unverified Data**)
40% Mineral Reinforced Polyamide 66 Minlon 11C40 NC010 is a 40% mineral reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Tensile Stress 81.2 MPa

@Strain 5.50 %,
Temperature 90.0 °C
11800 psi

@Strain 5.50 %,
Temperature 194 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 73G30T NC010 Nylon 6  (Unverified Data**)
30% Glass Reinforced Toughened Polyamide 6 Zytel 73G30T NC010 is a 30% glass fiber reinforced toughened polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers
Tensile Stress 81.3 MPa

@Strain 3.86 %,
Temperature 150 °C
11800 psi

@Strain 3.86 %,
Temperature 302 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 73G45L NC010 Nylon 6  (Unverified Data**)
45% Glass Reinforced Polyamide 6Zytel 73G45L NC010 is a 45% glass fiber reinforced polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers